The preshipment inspections of tableware are very important to make sure all safety requirements, PO stipulations, production specifications are met. The quality checks will mostly follow below methods:
INSPECTION CHECKPOINTS | RESULTS | COMMENTS |
---|---|---|
A. Quantity check | OK | |
B. Shipping marks & packing | NOT OK | |
C. Labels, logos and colors | OK | |
D. Styles & measurements | OK | |
E. Onsite safety and function tests | OK | |
F. Special requirements | OK | |
G. AQL workmanship (Visual checks) |
OK |
As the quality control inspections can happen at any stage of manufacturing, so there are:
The checklist for onsite quality inspection test will be like below:
INSPECTION CHECK LIST | COMMENTS | RESULT |
---|---|---|
Perform a fitting test check-The lid should fit the base well.-II | PASSED | |
Check capacity (volume) by weighing the item or by using a capacity gauge ( the mug, bowl and the container claimed with the volumn)-The results must conform with the specifications.-S2 | FAILED | |
Compare the inspection sample with the approval sample.-II | PASSED | |
Test the fit of the lid. and lid can not falls off when the teapot is tilted toward 90 degrees-If the item has a lid - The lid should fit well.-S3 | PASSED | |
If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-S2 |
PASSED | |
Test the item for water leakage during the entire inspection period.-Fill the item with water then place onto a paper to check there is no leakage at all.-S2 | FAILED | |
Test the strength of the handle.--S2 | PASSED | |
Hand washing test -- --Wash the product with cotton fabric in cold water of room temperature (about 20--35degree) and hot water of tempertature (about 80 -- 90 degree) -- During washing, dip product into the water and wiping the whole surface of the product -No color should be removed from the item’s surface during the test and no printing, markings or paint should fade.-3 pcs | PASSED | |
Check if items stand properly when pieces are stacked up, if this test fail, please state the cause clearly on inspection report and take photos- 1)Stack the products (60 pieces for the plate/reference and 12 pieces for bowl/reference and cup/reference ); 2) Ensure they can stack properly and do not wobble or tilt over-S2 |
PASSED | |
Perform a wobble test on a flat glass panel. Check both the top rim of the glass and the bottom.-There should be no wobbling of the base or the rim.-I | PASSED | |
Perform a fatigue test-On all adjustable parts. Do this 20 times.-S2 | PASSED |
tableware 3rd party inspection in China, China tableware third party inspection, tableware 3rd party inspection, China tableware 3rd party inspection services, tableware third party inspection in China, China tableware third party inspection services, tableware 3rd party inspection services, China tableware 3rd party inspection, tableware third party inspection services in China, China tableware third party inspection, tableware third party inspection, tableware third party inspection in China, tableware third party inspection services in China, tableware third party inspection services, tableware third party inspection services, tableware 3rd party inspection services in China, China tableware third party inspection services